Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 18.6 % Show Material materials with Dehnung of 18.6 % | Predicted Value, A80 | |||
18.9 % Show Material materials with Dehnung of 18.9 % | Predicted Value, Transverse | ||||
19 % Show Material materials with Dehnung of 19 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A200 | |
19.9 % Show Material materials with Dehnung of 19.9 % | Predicted Value, A80 Transverse | ||||
23 % Show Material materials with Dehnung of 23 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A50 | |
23.7 % Show Material materials with Dehnung of 23.7 % | Predicted Value | ||||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | |||
Flächenreduzierung | 42.7 % Show Material materials with Flächenreduzierung of 42.7 % | Predicted Value | |||
43.0 % Show Material materials with Flächenreduzierung of 43.0 % | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | |||
Scherfestigkeit | 505.7 MPa Show Material materials with Scherfestigkeit of 505.7 MPa | Predicted Value | |||
Schubmodule | 79.6 GPa Show Material materials with Schubmodule of 79.6 GPa | Predicted Value | |||
Zugfestigkeit | 450 - 585 MPa Show Material materials with Zugfestigkeit of 450 - 585 MPa | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.83 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.83 1/K | Predicted Value |
Spezifische Wärmekapazität | 457.4 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 457.4 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 39.62 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 39.62 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.24 % Show Material materials with Kohlenstoff of 0.24 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Mangan | 0.85 - 1.2 % Show Material materials with Mangan of 0.85 - 1.2 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |