Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 20 - 30 % Show Material materials with Dehnung A50 of 20 - 30 % |
Kerbschlagenergie | 23.0 °C | 18 J Show Material materials with Kerbschlagenergie of 18 J |
Streckgrenze | 23.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa |
Zugfestigkeit | 23.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.19 % Show Material materials with Kohlenstoff of 0.19 % |
Mangan | 0.31 - 0.64 % Show Material materials with Mangan of 0.31 - 0.64 % |
Nickel | 3.18 - 3.82 % Show Material materials with Nickel of 3.18 - 3.82 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.18 - 0.37 % Show Material materials with Silizium of 0.18 - 0.37 % |