Kohlenstoffarmer Stahl
EN 10028-2 Grade P295GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-2 Grade P355GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10120 Grade P265NB normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Steel
ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Nickel Chromium Molybdenum Steel
Carbodur 6587 Blank HardenedGeliefert von:
Deutsche Edelstahlwerke (DEW)Kohlenstoffarmer Stahl
EN 10216-2 Grade 19Mn5 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17200 Grade C22 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17243 Grade C22.8 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10250-2 Grade 20Mn5 quenched and tempered (+QT)