Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 16.4 % Show Material materials with Dehnung of 16.4 % | Predicted Value, A200 | |||
18.4 % Show Material materials with Dehnung of 18.4 % | Predicted Value, Transverse | ||||
20 % Show Material materials with Dehnung of 20 % | Double-Normalized and Tempered | ASTM A353 | Plate | A50 | |
21.1 % Show Material materials with Dehnung of 21.1 % | Predicted Value | ||||
22.2 % Show Material materials with Dehnung of 22.2 % | Predicted Value, A80 | ||||
29.0 % Show Material materials with Dehnung of 29.0 % | Predicted Value, A80 Transverse | ||||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel | |||
Flächenreduzierung | 42.6 % Show Material materials with Flächenreduzierung of 42.6 % | Predicted Value, Transverse | |||
44.7 % Show Material materials with Flächenreduzierung of 44.7 % | Predicted Value | ||||
Poissonzahl | 0.291 [-] Show Material materials with Poissonzahl of 0.291 [-] | Typical for Nickel Steel | |||
Scherfestigkeit | 581.2 MPa Show Material materials with Scherfestigkeit of 581.2 MPa | Predicted Value | |||
Schubmodule | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel | |||
Zugfestigkeit | 690 - 825 MPa Show Material materials with Zugfestigkeit of 690 - 825 MPa | Double-Normalized and Tempered | ASTM A353 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 12.25 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 12.25 1/K | Predicted Value |
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel |
Spezifische Wärmekapazität | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.13 % Show Material materials with Kohlenstoff of 0.13 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Mangan | 0.9 % Show Material materials with Mangan of 0.9 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Nickel | 8.5 - 9.5 % Show Material materials with Nickel of 8.5 - 9.5 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Phosphor | 0.015 % Show Material materials with Phosphor of 0.015 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | Double-Normalized and Tempered | ASTM A353 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |