Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 86 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 86 [-] | |
Härte, Vickers | 23.0 °C | 160 [-] Show Material materials with Härte, Vickers of 160 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 220 MPa Show Material materials with Streckgrenze Rp 0,2 of 220 MPa | |
Zugfestigkeit | 23.0 °C | 580 MPa Show Material materials with Zugfestigkeit of 580 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kobalt | 0.5 % Show Material materials with Kobalt of 0.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Molybdän | 3.5 - 6 % Show Material materials with Molybdän of 3.5 - 6 % |
Nickel | 79 - 82 % Show Material materials with Nickel of 79 - 82 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |