Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 22 % Show Material materials with Dehnung A50 of 22 % |
Flächenreduzierung | 23.0 °C | 35 % Show Material materials with Flächenreduzierung of 35 % |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.4 - 0.7 % Show Material materials with Chrom of 0.4 - 0.7 % |
Kohlenstoff | 0.25 % Show Material materials with Kohlenstoff of 0.25 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Molybdän | 0.4 - 0.6 % Show Material materials with Molybdän of 0.4 - 0.6 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |