Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Härte, Brinell | 23.0 °C | 202 - 273 [-] Show Material materials with Härte, Brinell of 202 - 273 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Zugfestigkeit | 23.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 4.5 - 5.5 % Show Material materials with Chrom of 4.5 - 5.5 % |
Kohlenstoff | 2.6 % Show Material materials with Kohlenstoff of 2.6 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 28 - 32 % Show Material materials with Nickel of 28 - 32 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Silizium | 5 - 6 % Show Material materials with Silizium of 5 - 6 % |