Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 17.9 % Show Material materials with Dehnung of 17.9 % | Predicted Value, A80 | |||
18 % Show Material materials with Dehnung of 18 % | Normalized | ASTM A537 | Plate | A200 | |
18.5 % Show Material materials with Dehnung of 18.5 % | Predicted Value, Transverse | ||||
19.3 % Show Material materials with Dehnung of 19.3 % | Predicted Value, A80 Transverse | ||||
22 % Show Material materials with Dehnung of 22 % | Normalized | ASTM A537 | Plate | A50 | |
24.7 % Show Material materials with Dehnung of 24.7 % | Predicted Value | ||||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | |||
Flächenreduzierung | 40.6 % Show Material materials with Flächenreduzierung of 40.6 % | Predicted Value | |||
43.9 % Show Material materials with Flächenreduzierung of 43.9 % | Predicted Value, Transverse | ||||
Härte, Brinell | 239 [-] Show Material materials with Härte, Brinell of 239 [-] | Predicted Value, Transverse | |||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | |||
Scherfestigkeit | 534.1 MPa Show Material materials with Scherfestigkeit of 534.1 MPa | Predicted Value | |||
Schubmodule | 79.6 GPa Show Material materials with Schubmodule of 79.6 GPa | Predicted Value | |||
Streckgrenze | 264.2 MPa Show Material materials with Streckgrenze of 264.2 MPa | Predicted Value, RP1 | |||
310 MPa Show Material materials with Streckgrenze of 310 MPa | Normalized | ASTM A537 | Plate | ||
317.5 MPa Show Material materials with Streckgrenze of 317.5 MPa | Predicted Value, RP1 Transverse | ||||
338.9 MPa Show Material materials with Streckgrenze of 338.9 MPa | Predicted Value, RP05 | ||||
345 MPa Show Material materials with Streckgrenze of 345 MPa | Normalized | ASTM A537 | Plate | ||
345.4 MPa Show Material materials with Streckgrenze of 345.4 MPa | Predicted Value, Transverse | ||||
378 MPa Show Material materials with Streckgrenze of 378 MPa | Predicted Value, RP02 | ||||
404.9 MPa Show Material materials with Streckgrenze of 404.9 MPa | Predicted Value, RP002 | ||||
469.4 MPa Show Material materials with Streckgrenze of 469.4 MPa | Predicted Value, RP02 Transverse | ||||
Zugfestigkeit | 450 - 585 MPa Show Material materials with Zugfestigkeit of 450 - 585 MPa | Normalized | ASTM A537 | Plate | |
485 - 620 MPa Show Material materials with Zugfestigkeit of 485 - 620 MPa | Normalized | ASTM A537 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.94 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.94 1/K | Predicted Value |
Spezifische Wärmekapazität | 458 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 458 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 32.64 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 32.64 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | Normalized | ASTM A537 | Plate |
Kohlenstoff | 0.24 % Show Material materials with Kohlenstoff of 0.24 % | Normalized | ASTM A537 | Plate |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % | Normalized | ASTM A537 | Plate |
Mangan | 0.7 - 1.35 % Show Material materials with Mangan of 0.7 - 1.35 % | Normalized | ASTM A537 | Plate |
Molybdän | 0.08 % Show Material materials with Molybdän of 0.08 % | Normalized | ASTM A537 | Plate |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % | Normalized | ASTM A537 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Normalized | ASTM A537 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | Normalized | ASTM A537 | Plate |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % | Normalized | ASTM A537 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |