Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 43 % Show Material materials with Flächenreduzierung of 43 % | |
Kerbschlagenergie | 23.0 °C | 54 J Show Material materials with Kerbschlagenergie of 54 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 895 - 1035 MPa Show Material materials with Streckgrenze Rp 0,2 of 895 - 1035 MPa | |
Yield strength Rp0.02 | 23.0 °C | 860 - 1000 MPa Show Material materials with Yield strength Rp0.02 of 860 - 1000 MPa | |
Zugfestigkeit | 23.0 °C | 965 MPa Show Material materials with Zugfestigkeit of 965 MPa |