Kohlenstoffarmer Stahl
EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 18MnMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Carbon Steel
ASTM A516 Grade 380 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A542 Type B Class 1 Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Unclassified Carbon Steel
ASTM A516 Grade 450 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Unclassified Carbon Steel
ASTM A516 Grade 415 As-Rolled or Normalized and/or Stress RelievedGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
DIN 17200 Grade C22 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C35E quenched and tempered (+QT)