Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 16 % Show Material materials with Dehnung A50 of 16 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Härte, Brinell | 23.0 °C | 277 [-] Show Material materials with Härte, Brinell of 277 [-] | |
Härte, Rockwell C | 23.0 °C | 28 [-] Show Material materials with Härte, Rockwell C of 28 [-] | |
Kerbschlagenergie | 23.0 °C | 41 J Show Material materials with Kerbschlagenergie of 41 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 725 MPa Show Material materials with Streckgrenze of 725 MPa | |
Zugfestigkeit | 23.0 °C | 930 MPa Show Material materials with Zugfestigkeit of 930 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 17.5 % Show Material materials with Chrom of 15 - 17.5 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Kupfer | 3 - 5 % Show Material materials with Kupfer of 3 - 5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 3 - 5 % Show Material materials with Nickel of 3 - 5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |