Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Elongation A200 | 23.0 °C | 25 % Show Material materials with Elongation A200 of 25 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp0,5 | 23.0 °C | 195 MPa Show Material materials with Streckgrenze Rp0,5 of 195 MPa | |
Zugfestigkeit | 23.0 °C | 345 - 450 MPa Show Material materials with Zugfestigkeit of 345 - 450 MPa |