Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 235 [-] Show Material materials with Härte, Brinell of 235 [-] | |
Härte, Rockwell B | 23.0 °C | 99 [-] Show Material materials with Härte, Rockwell B of 99 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa | |
Zugfestigkeit | 23.0 °C | 690 MPa Show Material materials with Zugfestigkeit of 690 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 11.5 - 13.5 % Show Material materials with Chrom of 11.5 - 13.5 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 1.25 - 2.5 % Show Material materials with Nickel of 1.25 - 2.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |