Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.83 g/cm³ Show Material materials with Dichte of 7.83 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 15 % Show Material materials with Dehnung of 15 % | Annealed |
Elastizitätsmodul | 23.0 °C | 212 GPa Show Material materials with Elastizitätsmodul of 212 GPa | |
Härte, Rockwell B | 23.0 °C | 90 [-] Show Material materials with Härte, Rockwell B of 90 [-] | Annealed |
Härte, Vickers | 23.0 °C | 340 - 490 [-] Show Material materials with Härte, Vickers of 340 - 490 [-] | Quenched and Tempered - Annealed: Max=195 |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 480 MPa Show Material materials with Streckgrenze Rp 0,2 of 480 MPa | Annealed |
Zugfestigkeit | 23.0 °C | 1100 - 1600 MPa Show Material materials with Zugfestigkeit of 1100 - 1600 MPa | Quenched and Tempered condition - Annealed condition: Max=620 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.15E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.15E-5 1/K | |
100.0 °C | 1.21E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.21E-5 1/K | ||
200.0 °C | 1.27E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.27E-5 1/K | ||
300.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | ||
400.0 °C | 1.36E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.36E-5 1/K | ||
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 20.0 °C | 45.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 45.1 W/(m·K) | |
200.0 °C | 44.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44.1 W/(m·K) | ||
300.0 °C | 41.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 41.9 W/(m·K) | ||
400.0 °C | 39.4 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 39.4 W/(m·K) | ||
500.0 °C | 36.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36.9 W/(m·K) | ||
Chemical properties
Property | Value |
---|---|
Chrom | 0.9 - 1.2 % Show Material materials with Chrom of 0.9 - 1.2 % |
Kohlenstoff | 0.38 - 0.45 % Show Material materials with Kohlenstoff of 0.38 - 0.45 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Molybdän | 0.15 - 0.25 % Show Material materials with Molybdän of 0.15 - 0.25 % |
Silizium | 0.17 - 0.37 % Show Material materials with Silizium of 0.17 - 0.37 % |