Stockholder of special alloys, Manufacturer of CNC machined fasteners
Headquarters
Sheffield, United Kingdom
Website
Type
Manufacturer, Processor and Distributor
Certifications
ISO 9001
, PED
, AD 2000
Grade | Shape | ||
---|---|---|---|
10.9/10 | Rod | EN ISO 898-1, EN ISO 898-2 | |
12.9/12 | Rod | EN ISO 898-1, EN ISO 898-2 | |
ASTM A193 Grade B7 | Rod, Bar, Fastener | ASTM A193 Grade B7, ASTM A320 Grade L7 | ASTM A193, ASTM A320 |
DSTAN 02-862 PT3 ISS3 | Rod | SM 1-M, SM 1-U, SM 2-M, SM 20U | |
Durehete 1055 | Rod | EN 1.7729 | |
Durehete 950 | Rod | EN 1.7711 | |
EN 1.4913 | Rod | EN X19CrMoNbVN11-1, Jethete X19 | EN 10269 |
EN 1.4923 | Rod | EN X22CrMoV12-1 | EN 10269 |
EN 1.4980 | Rod | EN X6NiCrTiMoVB25-15-2 | EN 10269 |
EN 1.4986 | Rod | EN X7CrNiMoBNb16-16 | EN 10269 |