Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 21 % Show Material materials with Dehnung A50 of 21 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 345 MPa Show Material materials with Streckgrenze Rp 0,2 of 345 MPa | |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.4 - 0.65 % Show Material materials with Chrom of 0.4 - 0.65 % |
Kohlenstoff | 0.19 % Show Material materials with Kohlenstoff of 0.19 % |
Kupfer | 0.25 - 0.4 % Show Material materials with Kupfer of 0.25 - 0.4 % |
Mangan | 0.8 - 1.25 % Show Material materials with Mangan of 0.8 - 1.25 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.3 - 0.65 % Show Material materials with Silizium of 0.3 - 0.65 % |
Vanadium | 0.02 - 0.1 % Show Material materials with Vanadium of 0.02 - 0.1 % |