Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Dichte of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Härte, Brinell | 23.0 °C | 217 [-] Show Material materials with Härte, Brinell of 217 [-] | |
Härte, Rockwell B | 23.0 °C | 95 [-] Show Material materials with Härte, Rockwell B of 95 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 290 MPa Show Material materials with Streckgrenze Rp 0,2 of 290 MPa | |
Zugfestigkeit | 23.0 °C | 600 MPa Show Material materials with Zugfestigkeit of 600 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 18 - 19 % Show Material materials with Chrom of 18 - 19 % |
Kohlenstoff | 0.04 - 0.06 % Show Material materials with Kohlenstoff of 0.04 - 0.06 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Nickel | 9 - 10 % Show Material materials with Nickel of 9 - 10 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 - 2 % Show Material materials with Silizium of 1 - 2 % |
Stickstoff | 0.12 - 0.18 % Show Material materials with Stickstoff of 0.12 - 0.18 % |