Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 250 [-] Show Material materials with Härte, Brinell of 250 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 430 MPa Show Material materials with Streckgrenze Rp 0,2 of 430 MPa | |
Zugfestigkeit | 23.0 °C | 750 MPa Show Material materials with Zugfestigkeit of 750 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 25 % Show Material materials with Chrom of 24 - 25 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.3 - 0.6 % Show Material materials with Kupfer of 0.3 - 0.6 % |
Mangan | 2 - 4 % Show Material materials with Mangan of 2 - 4 % |
Molybdän | 7 - 8 % Show Material materials with Molybdän of 7 - 8 % |
Nickel | 21 - 23 % Show Material materials with Nickel of 21 - 23 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 5E-3 % Show Material materials with Schwefel of 5E-3 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.45 - 0.55 % Show Material materials with Stickstoff of 0.45 - 0.55 % |