Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Streckgrenze | 23.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa | |
Zugfestigkeit | 23.0 °C | 520 MPa Show Material materials with Zugfestigkeit of 520 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 19.5 - 23.5 % Show Material materials with Chrom of 19.5 - 23.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 1.5 - 3.5 % Show Material materials with Kupfer of 1.5 - 3.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 2.5 - 3.5 % Show Material materials with Molybdän of 2.5 - 3.5 % |
Nickel | 38 - 44 % Show Material materials with Nickel of 38 - 44 % |
Niobium | 0.6 - 1.2 % Show Material materials with Niobium of 0.6 - 1.2 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |