Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 55 % Show Material materials with Flächenreduzierung of 55 % | |
Härte, Brinell | 23.0 °C | 255 [-] Show Material materials with Härte, Brinell of 255 [-] | |
Härte, Rockwell C | 23.0 °C | 24 [-] Show Material materials with Härte, Rockwell C of 24 [-] | |
Kerbschlagenergie | 23.0 °C | 75 J Show Material materials with Kerbschlagenergie of 75 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 520 MPa Show Material materials with Streckgrenze Rp 0,2 of 520 MPa | |
Zugfestigkeit | 23.0 °C | 795 MPa Show Material materials with Zugfestigkeit of 795 MPa |