Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Dehnung A50, transversal | 23.0 °C | 6 % Show Material materials with Dehnung A50, transversal of 6 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Flächenreduzierung, transversal | 23.0 °C | 25 % Show Material materials with Flächenreduzierung, transversal of 25 % | |
Hardness, Brinell, trans | 23.0 °C | 363 [-] Show Material materials with Hardness, Brinell, trans of 363 [-] | |
Härte, Brinell | 23.0 °C | 363 [-] Show Material materials with Härte, Brinell of 363 [-] | |
Härte, Rockwell C | 23.0 °C | 40 [-] Show Material materials with Härte, Rockwell C of 40 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 1275 MPa Show Material materials with Streckgrenze Rp 0,2 of 1275 MPa | |
Streckgrenze Rp 0,2, transversal | 23.0 °C | 1275 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 1275 MPa | |
Zugfestigkeit | 23.0 °C | 1410 MPa Show Material materials with Zugfestigkeit of 1410 MPa | |
Zugfestigkeit, transversal | 23.0 °C | 1410 MPa Show Material materials with Zugfestigkeit, transversal of 1410 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 14 - 16 % Show Material materials with Chrom of 14 - 16 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 1.25 - 1.75 % Show Material materials with Kupfer of 1.25 - 1.75 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.5 - 1 % Show Material materials with Molybdän of 0.5 - 1 % |
Nickel | 5 - 7 % Show Material materials with Nickel of 5 - 7 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |