Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 25 - 35 % Show Material materials with Dehnung A50 of 25 - 35 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Streckgrenze | 23.0 °C | 170 MPa Show Material materials with Streckgrenze of 170 MPa | |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.15 - 0.6 % Show Material materials with Aluminium of 0.15 - 0.6 % |
Chrom | 25 - 29 % Show Material materials with Chrom of 25 - 29 % |
Kohlenstoff | 0.06 - 0.1 % Show Material materials with Kohlenstoff of 0.06 - 0.1 % |
Kupfer | 0.75 % Show Material materials with Kupfer of 0.75 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 32 - 37 % Show Material materials with Nickel of 32 - 37 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 0.15 - 0.6 % Show Material materials with Titan of 0.15 - 0.6 % |