Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 - 30 % Show Material materials with Dehnung A50 of 20 - 30 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Kerbschlagenergie | 23.0 °C | 17.6 J Show Material materials with Kerbschlagenergie of 17.6 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa | |
Zugfestigkeit | 23.0 °C | 450 - 620 MPa Show Material materials with Zugfestigkeit of 450 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Mangan | 0.31 - 0.64 % Show Material materials with Mangan of 0.31 - 0.64 % |
Nickel | 3.2 - 3.8 % Show Material materials with Nickel of 3.2 - 3.8 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Silizium | 0.13 - 0.37 % Show Material materials with Silizium of 0.13 - 0.37 % |