Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Härte, Brinell | 23.0 °C | 256 [-] Show Material materials with Härte, Brinell of 256 [-] | |
Härte, Rockwell B | 23.0 °C | 100 [-] Show Material materials with Härte, Rockwell B of 100 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Streckgrenze | 23.0 °C | 330 MPa Show Material materials with Streckgrenze of 330 MPa | |
Zugfestigkeit | 23.0 °C | 675 MPa Show Material materials with Zugfestigkeit of 675 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 22 - 24 % Show Material materials with Chrom of 22 - 24 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 6 - 6.8 % Show Material materials with Molybdän of 6 - 6.8 % |
Nickel | 20 - 23 % Show Material materials with Nickel of 20 - 23 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.21 - 0.32 % Show Material materials with Stickstoff of 0.21 - 0.32 % |