Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 17.1 % Show Material materials with Dehnung of 17.1 % | Predicted Value, A200 | ||||
21.8 % Show Material materials with Dehnung of 21.8 % | Predicted Value, A5 | |||||
23.2 % Show Material materials with Dehnung of 23.2 % | Predicted Value, A50 | |||||
20 °C | 12 % Show Material materials with Dehnung of 12 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 Transverse | |
20 °C | 13 % Show Material materials with Dehnung of 13 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 Transverse | |
20 °C | 14 % Show Material materials with Dehnung of 14 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 Transverse | |
20 °C | 15 % Show Material materials with Dehnung of 15 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 Transverse | |
20 °C | 16 % Show Material materials with Dehnung of 16 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 Transverse | |
20 °C | 16 % Show Material materials with Dehnung of 16 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 | |
20 °C | 17 % Show Material materials with Dehnung of 17 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 | |
20 °C | 18 % Show Material materials with Dehnung of 18 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | A80 | |
20 °C | 20 % Show Material materials with Dehnung of 20 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Flat, Bar, Sheet, Strip | Transverse | |
20 °C | 22 % Show Material materials with Dehnung of 22 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Flat, Bar, Sheet, Strip | ||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Flächenreduzierung | 41.0 % Show Material materials with Flächenreduzierung of 41.0 % | Predicted Value | ||||
43.7 % Show Material materials with Flächenreduzierung of 43.7 % | Predicted Value, Transverse | |||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | ||||
Scherfestigkeit | 513.2 MPa Show Material materials with Scherfestigkeit of 513.2 MPa | Predicted Value | ||||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||||
Streckgrenze | 254.2 MPa Show Material materials with Streckgrenze of 254.2 MPa | Predicted Value, RP1 | ||||
316.5 MPa Show Material materials with Streckgrenze of 316.5 MPa | Predicted Value, RP1 Transverse | |||||
350.6 MPa Show Material materials with Streckgrenze of 350.6 MPa | Predicted Value, Transverse | |||||
355.9 MPa Show Material materials with Streckgrenze of 355.9 MPa | Predicted Value, RP02 | |||||
366.5 MPa Show Material materials with Streckgrenze of 366.5 MPa | Predicted Value, RP05 | |||||
446.5 MPa Show Material materials with Streckgrenze of 446.5 MPa | Predicted Value, RP02 Transverse | |||||
482.8 MPa Show Material materials with Streckgrenze of 482.8 MPa | Predicted Value, RP002 | |||||
20 °C | 345 MPa Show Material materials with Streckgrenze of 345 MPa | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat | ||
20 °C | 355 MPa Show Material materials with Streckgrenze of 355 MPa | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat | ||
Zugfestigkeit | 20 °C | 490 - 630 MPa Show Material materials with Zugfestigkeit of 490 - 630 MPa | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat | |
20 °C | 490 - 680 MPa Show Material materials with Zugfestigkeit of 490 - 680 MPa | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | ||
20 °C | 510 - 680 MPa Show Material materials with Zugfestigkeit of 510 - 680 MPa | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat | ||
20 °C | 510 - 630 MPa Show Material materials with Zugfestigkeit of 510 - 630 MPa | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Sheet, Strip, Flat |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel | |||
Max. Betriebstemperatur | -20 °C Show Material materials with Max. Betriebstemperatur of -20 °C | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat | Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | ||||
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel | |||
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel | |||
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 8 S/m Show Material materials with Elektrische Leitfähigkeit of 8 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat |
Mangan | 1.6 % Show Material materials with Mangan of 1.6 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat |
Silizium | 0.55 % Show Material materials with Silizium of 0.55 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat |
Stickstoff | 0.009 % Show Material materials with Stickstoff of 0.009 % | as-rolled condition (+AR) | EN 10025, EN 10025-1, EN 10025-2 | Bar, Sheet, Strip, Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |