Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J0C as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S235JR as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade E295 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
DIN 17103 Grade TStE 285 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S235JRG2C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235J0C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S275J2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S355J2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S355K2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S235J2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S275J2G4C normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S355J2G4C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S355K2G4C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S275J0C as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S275JRC as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235JRG1 as-rolled condition (+AR)Kohlenstoffarmer Stahl
DIN 17103 Grade WStE 285 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17103 Grade WStE 355 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S235JRC as-rolled condition (+AR)Kohlenstoffarmer Stahl
EN 10025 Grade S235J2G4C as-rolled condition (+AR)