Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 20.0 °C | 22.0 % Show Material materials with Dehnung of 22.0 % | thermomechanically rolled | EN 10225 | Sheet | |
Elastizitätsmodul | 190.0 - 210.0 GPa Show Material materials with Elastizitätsmodul of 190.0 - 210.0 GPa | Typical for Steel | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Streckgrenze | 20.0 °C | 325.0 MPa Show Material materials with Streckgrenze of 325.0 MPa | thermomechanically rolled | EN 10225 | Sheet | |
20.0 °C | 335.0 MPa Show Material materials with Streckgrenze of 335.0 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20.0 °C | 345.0 MPa Show Material materials with Streckgrenze of 345.0 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20.0 °C | 355.0 MPa Show Material materials with Streckgrenze of 355.0 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Zugfestigkeit | 20.0 °C | 470.0 - 630.0 MPa Show Material materials with Zugfestigkeit of 470.0 - 630.0 MPa | thermomechanically rolled | EN 10225 | Sheet |
Thermisch
Property | Value |
---|
Elektrisch
Property | Value |
---|
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.015 - 0.055 % Show Material materials with Aluminium of 0.015 - 0.055 % | thermomechanically rolled | EN 10225 | Sheet |
Antimon | 0.01 Show Material materials with Antimon of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Arsen | 0.03 Show Material materials with Arsen of 0.03 | thermomechanically rolled | EN 10225 | Sheet |
Bismut | 0.01 Show Material materials with Bismut of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Blei | 0.01 Show Material materials with Blei of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Bor | 0.001 Show Material materials with Bor of 0.001 | thermomechanically rolled | EN 10225 | Sheet |
Chrom | 0.25 Show Material materials with Chrom of 0.25 | thermomechanically rolled | EN 10225 | Sheet |
Kalzium | 0.005 Show Material materials with Kalzium of 0.005 | thermomechanically rolled | EN 10225 | Sheet |
Kohlenstoff | 0.14 Show Material materials with Kohlenstoff of 0.14 | thermomechanically rolled | EN 10225 | Sheet |
Kupfer | 0.3 Show Material materials with Kupfer of 0.3 | thermomechanically rolled | EN 10225 | Sheet |
Mangan | 1.0 - 1.65 % Show Material materials with Mangan of 1.0 - 1.65 % | thermomechanically rolled | EN 10225 | Sheet |
Molybdän | 0.08 Show Material materials with Molybdän of 0.08 | thermomechanically rolled | EN 10225 | Sheet |
Nickel | 0.5 Show Material materials with Nickel of 0.5 | thermomechanically rolled | EN 10225 | Sheet |
Niobium | 0.04 Show Material materials with Niobium of 0.04 | thermomechanically rolled | EN 10225 | Sheet |
Phosphor | 0.02 Show Material materials with Phosphor of 0.02 | thermomechanically rolled | EN 10225 | Sheet |
Schwefel | 0.01 Show Material materials with Schwefel of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Silizium | 0.15 - 0.55 % Show Material materials with Silizium of 0.15 - 0.55 % | thermomechanically rolled | EN 10225 | Sheet |
Stickstoff | 0.01 Show Material materials with Stickstoff of 0.01 | thermomechanically rolled | EN 10225 | Sheet |
Titan | 0.025 Show Material materials with Titan of 0.025 | thermomechanically rolled | EN 10225 | Sheet |
Vanadium | 0.06 Show Material materials with Vanadium of 0.06 | thermomechanically rolled | EN 10225 | Sheet |
Zinn | 0.02 Show Material materials with Zinn of 0.02 | thermomechanically rolled | EN 10225 | Sheet |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |