Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 15.1 % Show Material materials with Dehnung of 15.1 % | Predicted Value, A200 | ||||
15.2 % Show Material materials with Dehnung of 15.2 % | Predicted Value, A80 | |||||
18.1 % Show Material materials with Dehnung of 18.1 % | Predicted Value, Transverse | |||||
20.5 % Show Material materials with Dehnung of 20.5 % | Predicted Value, A5 | |||||
20.7 % Show Material materials with Dehnung of 20.7 % | Predicted Value, A80 Transverse | |||||
23.9 % Show Material materials with Dehnung of 23.9 % | Predicted Value, A50 | |||||
20 °C | 17 % Show Material materials with Dehnung of 17 % | thermomechanically rolled | EN 10225 | Sheet | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 39.8 % Show Material materials with Flächenreduzierung of 39.8 % | Predicted Value | ||||
44.4 % Show Material materials with Flächenreduzierung of 44.4 % | Predicted Value, Transverse | |||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 544.9 MPa Show Material materials with Scherfestigkeit of 544.9 MPa | Predicted Value | ||||
Schubmodule | 79.9 GPa Show Material materials with Schubmodule of 79.9 GPa | Predicted Value | ||||
Streckgrenze | 263.4 MPa Show Material materials with Streckgrenze of 263.4 MPa | Predicted Value, RP1 | ||||
318.6 MPa Show Material materials with Streckgrenze of 318.6 MPa | Predicted Value, RP1 Transverse | |||||
425.5 MPa Show Material materials with Streckgrenze of 425.5 MPa | Predicted Value, RP02 | |||||
431.2 MPa Show Material materials with Streckgrenze of 431.2 MPa | Predicted Value, Transverse | |||||
487.7 MPa Show Material materials with Streckgrenze of 487.7 MPa | Predicted Value, RP02 Transverse | |||||
500.1 MPa Show Material materials with Streckgrenze of 500.1 MPa | Predicted Value, RP05 | |||||
528 MPa Show Material materials with Streckgrenze of 528 MPa | Predicted Value, RP002 | |||||
20 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 405 MPa Show Material materials with Streckgrenze of 405 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 415 MPa Show Material materials with Streckgrenze of 415 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 420 MPa Show Material materials with Streckgrenze of 420 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 440 MPa Show Material materials with Streckgrenze of 440 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 460 MPa Show Material materials with Streckgrenze of 460 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Zugfestigkeit | 20 °C | 500 - 700 MPa Show Material materials with Zugfestigkeit of 500 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | |
20 °C | 500 - 690 MPa Show Material materials with Zugfestigkeit of 500 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 680 MPa Show Material materials with Zugfestigkeit of 500 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 675 MPa Show Material materials with Zugfestigkeit of 500 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 665 MPa Show Material materials with Zugfestigkeit of 500 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 660 MPa Show Material materials with Zugfestigkeit of 500 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 700 MPa Show Material materials with Zugfestigkeit of 505 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 690 MPa Show Material materials with Zugfestigkeit of 505 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 680 MPa Show Material materials with Zugfestigkeit of 505 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 675 MPa Show Material materials with Zugfestigkeit of 505 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 665 MPa Show Material materials with Zugfestigkeit of 505 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 660 MPa Show Material materials with Zugfestigkeit of 505 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 700 MPa Show Material materials with Zugfestigkeit of 515 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 690 MPa Show Material materials with Zugfestigkeit of 515 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 680 MPa Show Material materials with Zugfestigkeit of 515 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 675 MPa Show Material materials with Zugfestigkeit of 515 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 665 MPa Show Material materials with Zugfestigkeit of 515 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 660 MPa Show Material materials with Zugfestigkeit of 515 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 700 MPa Show Material materials with Zugfestigkeit of 520 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 690 MPa Show Material materials with Zugfestigkeit of 520 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 680 MPa Show Material materials with Zugfestigkeit of 520 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 675 MPa Show Material materials with Zugfestigkeit of 520 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 665 MPa Show Material materials with Zugfestigkeit of 520 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 660 MPa Show Material materials with Zugfestigkeit of 520 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 700 MPa Show Material materials with Zugfestigkeit of 530 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 690 MPa Show Material materials with Zugfestigkeit of 530 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 680 MPa Show Material materials with Zugfestigkeit of 530 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 675 MPa Show Material materials with Zugfestigkeit of 530 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 665 MPa Show Material materials with Zugfestigkeit of 530 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 660 MPa Show Material materials with Zugfestigkeit of 530 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 700 MPa Show Material materials with Zugfestigkeit of 540 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 690 MPa Show Material materials with Zugfestigkeit of 540 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 680 MPa Show Material materials with Zugfestigkeit of 540 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 675 MPa Show Material materials with Zugfestigkeit of 540 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 665 MPa Show Material materials with Zugfestigkeit of 540 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 660 MPa Show Material materials with Zugfestigkeit of 540 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.89 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.89 1/K | Predicted Value |
Spezifische Wärmekapazität | 453.1 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 453.1 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 37.03 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37.03 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.015 - 0.055 % Show Material materials with Aluminium of 0.015 - 0.055 % | thermomechanically rolled | EN 10225 | Sheet |
Antimon | 0.01 % Show Material materials with Antimon of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Arsen | 0.03 % Show Material materials with Arsen of 0.03 % | thermomechanically rolled | EN 10225 | Sheet |
Bismut | 0.01 % Show Material materials with Bismut of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Blei | 0.01 % Show Material materials with Blei of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Bor | 0.001 % Show Material materials with Bor of 0.001 % | thermomechanically rolled | EN 10225 | Sheet |
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | thermomechanically rolled | EN 10225 | Sheet |
Kalzium | 0.005 % Show Material materials with Kalzium of 0.005 % | thermomechanically rolled | EN 10225 | Sheet |
Kohlenstoff | 0.14 % Show Material materials with Kohlenstoff of 0.14 % | thermomechanically rolled | EN 10225 | Sheet |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | thermomechanically rolled | EN 10225 | Sheet |
Mangan | 1.65 % Show Material materials with Mangan of 1.65 % | thermomechanically rolled | EN 10225 | Sheet |
Molybdän | 0.25 % Show Material materials with Molybdän of 0.25 % | thermomechanically rolled | EN 10225 | Sheet |
Nickel | 0.7 % Show Material materials with Nickel of 0.7 % | thermomechanically rolled | EN 10225 | Sheet |
Niobium | 0.04 % Show Material materials with Niobium of 0.04 % | thermomechanically rolled | EN 10225 | Sheet |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % | thermomechanically rolled | EN 10225 | Sheet |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Silizium | 0.15 - 0.55 % Show Material materials with Silizium of 0.15 - 0.55 % | thermomechanically rolled | EN 10225 | Sheet |
Stickstoff | 0.01 % Show Material materials with Stickstoff of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Titan | 0.025 % Show Material materials with Titan of 0.025 % | thermomechanically rolled | EN 10225 | Sheet |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | thermomechanically rolled | EN 10225 | Sheet |
Zinn | 0.02 % Show Material materials with Zinn of 0.02 % | thermomechanically rolled | EN 10225 | Sheet |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |