CuNi10Fe1Mn (CW352H) is comparable to CuNi10Fe1Mn, mat. no. 2.0872, acc. to DIN 17664 : 1983-12. To the comparable DIN-mark applies: The material shows favorable specific strength values also at endurance loading and increased temperatures. Thermal conductivity of pure copper is strongly reduced by Ni, the electrical resistance strongly increases according to the Ni-content. Fe-addition increases the corrosion resistance. CuNi10Fe1Mn is resistant to seawater, alkaline saline solutions and non-oxidizing acids. warm forming: good cold forming: very good machinability: unfavorable hard soldering: very good soft soldering: very good gas-shielded welding: very good burnishing: good Application: For seawater pipilines, tubes and plates for all types of tubular heat-exchanger (condenser, cooler, seawater evaporators, high pressure feeder water heater) on ships, in power plants, seawater desalination plants, chemical and sugar factories.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.9 g/cm³

Show Material materials with Dichte of 8.9 g/cm³

Mechanisch

PropertyTemperatureValueComment

Elastizitätsmodul

23.0 °C

120 - 156 GPa

Show Material materials with Elastizitätsmodul of 120 - 156 GPa

Typical for Wrought Copper Nickel Grade

Härte, Brinell

20.0 °C

100 [-]

Show Material materials with Härte, Brinell of 100 [-]

Härte, Vickers

20.0 °C

100 - 105 [-]

Show Material materials with Härte, Vickers of 100 - 105 [-]

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

23.0 °C

1.4E-5 - 1.8E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 - 1.8E-5 1/K

Typical for Wrought Copper Nickel Grade

Schmelzpunkt

915 - 1240 °C

Show Material materials with Schmelzpunkt of 915 - 1240 °C

Typical for Wrought Copper Nickel Grade

Spezifische Wärmekapazität

20.0 °C

380 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K)

Wärmeleitfähigkeit

20.0 °C

50.2 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 50.2 W/(m·K)

Chemical properties

PropertyValue

Blei

0.02 %

Show Material materials with Blei of 0.02 %

Eisen

1 - 2 %

Show Material materials with Eisen of 1 - 2 %

Kobalt

0.1 %

Show Material materials with Kobalt of 0.1 %

Kohlenstoff

0.05 %

Show Material materials with Kohlenstoff of 0.05 %

Mangan

0.5 - 1 %

Show Material materials with Mangan of 0.5 - 1 %

Nickel

9 - 11 %

Show Material materials with Nickel of 9 - 11 %

Phosphor

0.02 %

Show Material materials with Phosphor of 0.02 %

Schwefel

0.05 %

Show Material materials with Schwefel of 0.05 %

Zink

0.5 %

Show Material materials with Zink of 0.5 %

Zinn

0.03 %

Show Material materials with Zinn of 0.03 %