About SARU COPPER

Saru Copper is an India-based leading manufacturer and exporter of copper rods, continuous cast and cold drawn copper alloy rods and copper alloy bars. We take pride that our products are being globally accepted since last several years for their quality and competitive pricing

Company profile

Headquarters

Meerut,Uttar Pradesh, India

Type

Manufacturer and Processor

Certifications

ISO 9001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN CuNi10Fe1Mn

Tube, Bar

EN CuNi10Fe1Mn, UNS C70600, EN CW352H

BS 2874 CN102, EN 12163, ASTM B121

EN CuNi12Zn24

Tube, Bar

EN CuNi12Zn24, UNS C75700, EN CW403J

BS 2870 NS 104, EN 12163, ASTM B151

EN CuSn10

Tube, Bar

EN CuSn10, JIS C5212

BS 1400 CT1, IS 28, DIN 17662, DIN 17672, ISO 427, JIS M-3270, ASTM B139

EN CuSn10P

Tube, Bar

EN CuSn10P

BS 1400 PB1, IS 28, DIN 1705, ISO 1338, ASTM B505

EN CuSn10Zn2

Tube, Bar

EN CuSn10Zn2

ASTM B505, BS 1400 G1, IS 306

EN CuSn11P

Tube, Bar

EN CuSn11P

BS 1400 PB2, IS 28, DIN 1705, ISO 1338, ASTM B505, AFNOR 53707

EN CuSn4Pb4Zn4

Tube, Bar

EN CuSn4Pb4Zn4, UNS C54400

ASTM B139

EN CuSn5

Tube, Bar

EN CuSn5, UNS C51000, JIS C5102

BS 2874, IS 7811, DIN 17662, DIN 17672, ISO 427, JIS H3270, ASTM B139

EN CuSn5Pb5Zn5

Tube, Bar

EN CuSn5Pb5Zn5, UNS C83600

ASTM B505, IS 1705, DIN 1338, BS 1400, ISO 318, SAE J461, SAE J462

EN CuSn6

Tube, Bar

EN CuSn6, UNS C51910, JIS C5191

BS 2875, BS 2870, PB-103, DIN 17662, DIN 17672, ISO 427, JIS H3270, ASTM H3270

Showing 1 to 10 of 15 entries

Previous

1
2

Next

Locations

India

India

Saru Nagar,Sardhana Road

250001 Meerut,Uttar Pradesh

(+91)9897026874