Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 - 8.88 g/cm³ Show Material materials with Dichte of 8.8 - 8.88 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 6 - 15 % Show Material materials with Dehnung of 6 - 15 % |
Dehnung A50 | 20.0 °C | 5 - 8 % Show Material materials with Dehnung A50 of 5 - 8 % |
Elastizitätsmodul | 20.0 °C | 130 - 143 GPa Show Material materials with Elastizitätsmodul of 130 - 143 GPa |
Elongation A10 | 20.0 °C | 5 - 8 % Show Material materials with Elongation A10 of 5 - 8 % |
Elongation A100 | 20.0 °C | 4 - 6 % Show Material materials with Elongation A100 of 4 - 6 % |
Härte, Brinell | 20.0 °C | 90 - 180 [-] Show Material materials with Härte, Brinell of 90 - 180 [-] |
Härte, Vickers | 20.0 °C | 95 - 220 [-] Show Material materials with Härte, Vickers of 95 - 220 [-] |
Poissonzahl | 20.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 230 - 620 MPa Show Material materials with Streckgrenze Rp 0,2 of 230 - 620 MPa |
Zugfestigkeit | 20.0 °C | 320 - 640 MPa Show Material materials with Zugfestigkeit of 320 - 640 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Spezifische Wärmekapazität | 20.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) |
Wärmeleitfähigkeit | 20.0 °C | 67 - 200 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 67 - 200 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.00E+7 - 2.60E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.00E+7 - 2.60E+7 S/m |
Specific Electrical conductivity | 29 - 45 % IACS Show Material materials with Specific Electrical conductivity of 29 - 45 % IACS |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 1.6 - 2.5 % Show Material materials with Nickel of 1.6 - 2.5 % |
Silizium | 0.4 - 0.8 % Show Material materials with Silizium of 0.4 - 0.8 % |