Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 10 % Show Material materials with Dehnung of 10 % |
Elongation A100 | 20.0 °C | 6 % Show Material materials with Elongation A100 of 6 % |
Härte, Vickers | 20.0 °C | 190 - 250 [-] Show Material materials with Härte, Vickers of 190 - 250 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 620 - 680 MPa Show Material materials with Streckgrenze Rp 0,2 of 620 - 680 MPa |
Zugfestigkeit | 20.0 °C | 640 - 700 MPa Show Material materials with Zugfestigkeit of 640 - 700 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Spezifische Wärmekapazität | 20.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 1.6 - 2.5 % Show Material materials with Nickel of 1.6 - 2.5 % |
Silizium | 0.4 - 0.8 % Show Material materials with Silizium of 0.4 - 0.8 % |