EN 12167 Grade CuNi2Si H150

View suppliers (8)
Want to keep this datasheet? Save it now in your required format

Description

CuNi2Si, mat. No CW111C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuBNi2Si, mat. No 2.0855, acc. to DIN 17666 : 1983-12 applies: The material shows favorable electrical and thermal conductivity, corrosion resistance, high fatigue and creep resistance as well as favorable spring properties. CuNi2Si is in hardened condition resistant to stress corrosion. Temperature for removal of workhardening approximates 450°C. Strength still increases at low-temperature range. Processing properties: hot and cold forming: good machinability: moderately soft soldering: good hard soldering: moderately gas shielded welding: moderately burnishing: good Application: Particularly for aerial line material, such as clamps, mounting links, nuts, high-strength and corrosion resistant screws. Furthermore for wire ropes in electrical overhead line construction, bearing bushings, roller bearing cages, valve guide bushings and springs. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.8 - 8.88 g/cm³

Show Material materials with Dichte of 8.8 - 8.88 g/cm³

Mechanisch

PropertyTemperatureValue

Elastizitätsmodul

20.0 °C

130 - 143 GPa

Show Material materials with Elastizitätsmodul of 130 - 143 GPa

Härte, Brinell

20.0 °C

150 - 190 [-]

Show Material materials with Härte, Brinell of 150 - 190 [-]

Poissonzahl

20.0 °C

0.34 [-]

Show Material materials with Poissonzahl of 0.34 [-]

Thermisch

PropertyTemperatureValue

Koeffizient der thermischen Ausdehnung

300.0 °C

1.6E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K

Spezifische Wärmekapazität

20.0 °C

377 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K)

Wärmeleitfähigkeit

20.0 °C

67 - 200 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 67 - 200 W/(m·K)

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

1.00E+7 - 2.60E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 1.00E+7 - 2.60E+7 S/m

Specific Electrical conductivity

34 - 45 % IACS

Show Material materials with Specific Electrical conductivity of 34 - 45 % IACS

Chemical properties

PropertyValue

Blei

0.02 %

Show Material materials with Blei of 0.02 %

Eisen

0.2 %

Show Material materials with Eisen of 0.2 %

Mangan

0.1 %

Show Material materials with Mangan of 0.1 %

Nickel

1.6 - 2.5 %

Show Material materials with Nickel of 1.6 - 2.5 %

Silizium

0.4 - 0.8 %

Show Material materials with Silizium of 0.4 - 0.8 %