Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.6 g/cm³ Show Material materials with Dichte of 7.6 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Härte, Brinell | 20.0 °C | 160 [-] Show Material materials with Härte, Brinell of 160 [-] | |
Härte, Vickers | 20.0 °C | 165 [-] Show Material materials with Härte, Vickers of 165 [-] | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Schubmodule | 20.0 °C | 43 GPa Show Material materials with Schubmodule of 43 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 20.0 °C | 377 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 418 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 57 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 57 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 7.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 7.00E+6 S/m |
Specific Electrical conductivity | 12.1 % IACS Show Material materials with Specific Electrical conductivity of 12.1 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Kupfer | 79.45 % Show Material materials with Kupfer of 79.45 % |
Mangan | 1.5 - 3.5 % Show Material materials with Mangan of 1.5 - 3.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |