About WMN Labedy

s part of the Nonferrous Metal (except Aluminum) Production and Processing Industr

Company profile

Headquarters

Gliwice, Śląskie, Poland

Type

Manufacturer and Processor

Certifications

ISO 9001

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN Cu99.7

Sheet

EN Cu99.7

EN 1652, EN 13599, DIN 1787, ASTM B152, JIS H3100, BS 2870

EN Cu99.9

Sheet

EN Cu99.9

EN 1652, EN 13599, DIN 1787, ASTM B152, JIS H3100, BS 2870

EN Cu99.95

Sheet

EN Cu99.95

EN 1652, EN 13599, DIN 1787, ASTM B152, JIS H3100, BS 2870

EN CuAl10Fe3Mn2

Sow

EN CuAl10Fe3Mn2, PN BA1032

PN-91/H-87026

EN CuAl10Fe4Ni4

Sow

EN CuAl10Fe4Ni4, PN BA1044

PN-91/H-87026

EN CuCrZr

Sheet

EN CuCrZr

DIN 17670-1, BS 2870

EN CuNi10

Sheet

EN CuNi10

EN 1652, ASTM C171, DIN 17670-1, BS 2870, JIS H3100

EN CuNi12Zn24

Strip, Sheet

EN CuNi12Zn24, EN MZN12

EN 1652, DIN 17663, ASTM B122, BS 2870

EN CuNi18Zn20

Strip, Sheet

EN CuNi18Zn20, EN MZ20N18

EN 1652, DIN 17663, ASTM B122, BS 2870

EN CuNi18Zn27

Strip, Sheet

EN CuNi18Zn27, EN MZN18

EN 1652, DIN 17663, ASTM B122, BS 2870