Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 46 % Show Material materials with Dehnung of 46 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 220 MPa Show Material materials with Streckgrenze of 220 MPa | |
Zugfestigkeit | 23.0 °C | 610 MPa Show Material materials with Zugfestigkeit of 610 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 450 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Bor | 1.5E-3 - 5E-3 % Show Material materials with Bor of 1.5E-3 - 5E-3 % |
Chrom | 17 - 19 % Show Material materials with Chrom of 17 - 19 % |
Eisen | 64 - 74 % Show Material materials with Eisen of 64 - 74 % |
Kohlenstoff | 0.04 - 0.1 % Show Material materials with Kohlenstoff of 0.04 - 0.1 % |
Mangan | 0 - 2 % Show Material materials with Mangan of 0 - 2 % |
Nickel | 9 - 13 % Show Material materials with Nickel of 9 - 13 % |
Phosphor | 0 - 0.05 % Show Material materials with Phosphor of 0 - 0.05 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |
Stickstoff | 0 - 0.1 % Show Material materials with Stickstoff of 0 - 0.1 % |
Titan | 0 - 0.8 % Show Material materials with Titan of 0 - 0.8 % |