Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 9.2 - 12 % Show Material materials with Dehnung of 9.2 - 12 % | |
Elastizitätsmodul | 23.0 °C | 210 GPa Show Material materials with Elastizitätsmodul of 210 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 1470 - 1740 MPa Show Material materials with Streckgrenze of 1470 - 1740 MPa | |
Zugfestigkeit | 23.0 °C | 1630 - 1860 MPa Show Material materials with Zugfestigkeit of 1630 - 1860 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 450 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 11 - 12.5 % Show Material materials with Chrom of 11 - 12.5 % |
Eisen | 71.5 - 79.2 % Show Material materials with Eisen of 71.5 - 79.2 % |
Kohlenstoff | 0 - 0.05 % Show Material materials with Kohlenstoff of 0 - 0.05 % |
Kupfer | 1.5 - 2.5 % Show Material materials with Kupfer of 1.5 - 2.5 % |
Mangan | 0 - 0.5 % Show Material materials with Mangan of 0 - 0.5 % |
Molybdän | 0 - 0.5 % Show Material materials with Molybdän of 0 - 0.5 % |
Nickel | 7.5 - 9.5 % Show Material materials with Nickel of 7.5 - 9.5 % |
Niobium | 0 - 0.5 % Show Material materials with Niobium of 0 - 0.5 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 0.5 % Show Material materials with Silizium of 0 - 0.5 % |
Tantal | 0 - 0.5 % Show Material materials with Tantal of 0 - 0.5 % |
Titan | 0.8 - 1.4 % Show Material materials with Titan of 0.8 - 1.4 % |