Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.15 g/cm³ Show Supplier Material materials with Dichte of 7.15 g/cm³ |
Molmasse | 52 g/mol Show Supplier Material materials with Molmasse of 52 g/mol |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 290 GPa Show Supplier Material materials with Elastizitätsmodul of 290 GPa |
Härte, Vickers, 10 | 23.0 °C | 180 - 250 [-] Show Supplier Material materials with Härte, Vickers, 10 of 180 - 250 [-] |
Poissonzahl | 23.0 °C | 0.21 [-] Show Supplier Material materials with Poissonzahl of 0.21 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.2E-6 1/K |
Schmelzpunkt | 1900 °C Show Supplier Material materials with Schmelzpunkt of 1900 °C | |
Siedepunkt | 2672 °C Show Supplier Material materials with Siedepunkt of 2672 °C | |
Spezifische Wärmekapazität | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 93.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 93.7 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 7.90E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 7.90E+6 S/m |
Elektronenaustrittsarbeit | 23.0 °C | 4.5 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.5 eV |
spezifischer Widerstand | 23.0 °C | 1.3E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.3E-7 Ω·m |
Akustisch
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.03 % Show Supplier Material materials with Andere of 0.03 % | ||
Chrom | 99.8 % Show Supplier Material materials with Chrom of 99.8 % | min | |
Eisen | 0.15 % Show Supplier Material materials with Eisen of 0.15 % | ||
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | ||
Molybdän | 0.005 | ||
Sauerstoff | 0.1 % Show Supplier Material materials with Sauerstoff of 0.1 % | ||
Silizium | 0.05 % Show Supplier Material materials with Silizium of 0.05 % | ||
Stickstoff | 0.02 % Show Supplier Material materials with Stickstoff of 0.02 % | ||
Wolfram | 5E-3 % Show Supplier Material materials with Wolfram of 5E-3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thanks to its very high corrosion resistance against many different acids and bases as well as hot gases, chromium is a popular material for all types of protective coating. In combustion equipment, chromium is used as a wear-resistant coating to increase the service life of specific components. As a component in high-temperature fuel cells, chromium also performs brilliantly. Alongside these applications, chromium is also used as a brilliant decorative coating for operating elements on appliances or for jewellery. |