Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Dichte of 10.2 g/cm³ |
Molmasse | 95.94 g/mol Show Supplier Material materials with Molmasse of 95.94 g/mol | |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 320 GPa Show Supplier Material materials with Elastizitätsmodul of 320 GPa | |
Härte, Vickers, 10 | 23.0 °C | 160 - 180 [-] Show Supplier Material materials with Härte, Vickers, 10 of 160 - 180 [-] | recrystallized |
Poissonzahl | 23.0 °C | 0.31 [-] Show Supplier Material materials with Poissonzahl of 0.31 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.2E-6 1/K |
Schmelzpunkt | 2620 °C Show Supplier Material materials with Schmelzpunkt of 2620 °C | |
Siedepunkt | 4639 °C Show Supplier Material materials with Siedepunkt of 4639 °C | |
Spezifische Wärmekapazität | 23.0 °C | 254 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 254 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 142 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 142 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.79E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.79E+7 S/m |
Elektronenaustrittsarbeit | 23.0 °C | 4.39 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.39 eV |
spezifischer Widerstand | 23.0 °C | 5.6E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.6E-8 Ω·m |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | 99.97 % Show Supplier Material materials with Molybdän of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 6E-4 % Show Supplier Material materials with Sauerstoff of 6E-4 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Molybdenum can be used, for example, to produce ribbons and wires for the lighting industry, semiconductor base plates for power electronics, glass melting electrodes, hot zones for high-temperature furnaces and sputtering targets for coating solar cells and flat screens. |