Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 1550 °C Show Supplier Material materials with Max. Betriebstemperatur of 1550 °C |
Chemical properties
Property | Value |
---|---|
Hafnium | 1.2 % Show Supplier Material materials with Hafnium of 1.2 % |
Kohlenstoff | 0.05 - 0.12 % Show Supplier Material materials with Kohlenstoff of 0.05 - 0.12 % |
Molybdän | balance |
Technological properties
Property | ||
---|---|---|
Application areas | MHC is used in metal forming applications, for example. When used in extrusion dies, it is able to withstand extreme thermal and mechanical loads. | |
Other | Molybdenum-hafnium carbide (MHC) is highly temperature-resistant, has a high level of thermal conductivity, a low coefficient of thermal expansion and a high recrystallization temperature. MHC retains its shape even when used at temperatures of up to 1550 °C. |