Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 19.3 g/cm³ Show Supplier Material materials with Dichte of 19.3 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 0.64 - 1 mm Show Supplier Material materials with Durchmesser of 0.64 - 1 mm |
Dimensions | Available diameters (mm): 0.635; 0.76; 1 |
Chemical properties
Property | Value |
---|---|
Aluminium | 3E-3 % Show Supplier Material materials with Aluminium of 3E-3 % |
Blei | 5E-4 % Show Supplier Material materials with Blei of 5E-4 % |
Cadmium | 5E-4 % Show Supplier Material materials with Cadmium of 5E-4 % |
Chrom | 2E-3 % Show Supplier Material materials with Chrom of 2E-3 % |
Eisen | 3E-3 % Show Supplier Material materials with Eisen of 3E-3 % |
Kalium | 3E-3 - 7E-3 % Show Supplier Material materials with Kalium of 3E-3 - 7E-3 % |
Kohlenstoff | 3E-3 % Show Supplier Material materials with Kohlenstoff of 3E-3 % |
Kupfer | 1E-3 % Show Supplier Material materials with Kupfer of 1E-3 % |
Molybdän | 0.01 % Show Supplier Material materials with Molybdän of 0.01 % |
Nickel | 2E-3 % Show Supplier Material materials with Nickel of 2E-3 % |
Quecksilber | 1E-4 % Show Supplier Material materials with Quecksilber of 1E-4 % |
Sauerstoff | 5E-3 % Show Supplier Material materials with Sauerstoff of 5E-3 % |
Silizium | 3E-3 % Show Supplier Material materials with Silizium of 3E-3 % |
Stickstoff | 1E-3 % Show Supplier Material materials with Stickstoff of 1E-3 % |
Wolfram | balance |
Technological properties
Property | ||
---|---|---|
Application areas | WVM is primarily supplied in rod or wire form for use in evaporation coils or heating filaments. |