Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 18.25 - 18.85 g/cm³ Show Supplier Material materials with Dichte of 18.25 - 18.85 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 30 - 70 mm Show Supplier Material materials with Durchmesser of 30 - 70 mm |
Länge | 250 - 500 mm Show Supplier Material materials with Länge of 250 - 500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 30 x 500; 40 x 500; 70 x 250 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % |
Härte, Vickers, 10 | 23.0 °C | 270 - 330 [-] Show Supplier Material materials with Härte, Vickers, 10 of 270 - 330 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 517 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 517 MPa |
Zugfestigkeit | 23.0 °C | 689 MPa Show Supplier Material materials with Zugfestigkeit of 689 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | 0.5 - 1.5 % Show Supplier Material materials with Eisen of 0.5 - 1.5 % |
Nickel | 1.5 - 2.5 % Show Supplier Material materials with Nickel of 1.5 - 2.5 % |
Wolfram | 96 - 98 % Show Supplier Material materials with Wolfram of 96 - 98 % |
Technological properties
Property | ||
---|---|---|
Application areas | Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Weakly ferromagnetic, DENSIMET® D185ND is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006. |