Allgemein
Property | Temperature | Value |
---|---|---|
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Thermisch
Property | Value |
---|---|
Kristallisationstemperatur | 900 - 1450 °C Show Supplier Material materials with Kristallisationstemperatur of 900 - 1450 °C |
Schmelzpunkt | 2966 °C Show Supplier Material materials with Schmelzpunkt of 2966 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.3 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.3 eV |
Supraleiterübergangstemperatur | -268.65 °C Show Supplier Material materials with Supraleiterübergangstemperatur of -268.65 °C |
Akustisch
Chemical properties
Property | Value | Comment |
---|---|---|
Tantal | 99.9 % Show Supplier Material materials with Tantal of 99.9 % | min |
Technological properties
Property | ||
---|---|---|
Application areas | Grain stabilized tantalum in the form of wire or sheets is ideal for sintering into tantalum anodes or for applications in the furnace construction sector. | |
Corrosion properties | Outstanding resistance against aqueous solutions and metal melts. | |
Other | This material has excellent cold ductility, superconductivity and a high level of biocompatibility. |