Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 18 g/cm³ Show Supplier Material materials with Dichte of 18 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 360 GPa Show Supplier Material materials with Elastizitätsmodul of 360 GPa |
Chemical properties
Property | Value |
---|---|
Kupfer | binder |
Nickel | binder |
Wolfram | 95 % Show Supplier Material materials with Wolfram of 95 % |
Technological properties
Property | ||
---|---|---|
Application areas | Inermet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Paramagnetic |