Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 16.6 g/cm³ Show Supplier Material materials with Dichte of 16.6 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Abmessung
Property | Value |
---|---|
Durchmesser | 4 - 10 mm Show Supplier Material materials with Durchmesser of 4 - 10 mm |
Länge | 300 - 2500 mm Show Supplier Material materials with Länge of 300 - 2500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 4 x 500-2000 ; 6 x 500-2500 ; 10 x 300-2500 |
Mechanisch
Thermisch
Property | Value |
---|---|
Kristallisationstemperatur | 900 - 1450 °C Show Supplier Material materials with Kristallisationstemperatur of 900 - 1450 °C |
Schmelzpunkt | 2966 °C Show Supplier Material materials with Schmelzpunkt of 2966 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.3 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.3 eV |
Supraleiterübergangstemperatur | -268.65 °C Show Supplier Material materials with Supraleiterübergangstemperatur of -268.65 °C |
Akustisch
Chemical properties
Property | Value | Comment |
---|---|---|
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % | |
Kohlenstoff | 1E-3 % Show Supplier Material materials with Kohlenstoff of 1E-3 % | |
Molybdän | 1E-3 % Show Supplier Material materials with Molybdän of 1E-3 % | |
Nickel | 5E-4 % Show Supplier Material materials with Nickel of 5E-4 % | |
Niobium | 1.9E-3 % Show Supplier Material materials with Niobium of 1.9E-3 % | |
Sauerstoff | 1.3E-3 % Show Supplier Material materials with Sauerstoff of 1.3E-3 % | |
Silizium | 1E-3 % Show Supplier Material materials with Silizium of 1E-3 % | |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % | |
Tantal | 99.95 % Show Supplier Material materials with Tantal of 99.95 % | min |
Titan | 1E-4 % Show Supplier Material materials with Titan of 1E-4 % | |
Wasserstoff | 4E-4 % Show Supplier Material materials with Wasserstoff of 4E-4 % | |
Wolfram | 2E-3 % Show Supplier Material materials with Wolfram of 2E-3 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Outstanding resistance against aqueous solutions and metal melts. | |
Other | This material has excellent cold ductility, superconductivity and a high level of biocompatibility. |