Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.15 g/cm³ Show Supplier Material materials with Dichte of 10.15 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Oberflächenrauigkeit | 0.8 - 1 μm Show Supplier Material materials with Oberflächenrauigkeit of 0.8 - 1 μm |
Abmessung
Property | Value |
---|---|
Durchmesser | 2 - 30 mm Show Supplier Material materials with Durchmesser of 2 - 30 mm |
Länge | 100 - 3000 mm Show Supplier Material materials with Länge of 100 - 3000 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 2 x 300-3000; 3 x 300-3000; 4 x 300-3000; 4.75 x 300-3000; 5 x 300-3000; 6 x 300-3000; 6.35 x 300-3000; 7 x 300-2900; 8 x 300-2900; 9 x 300-2900; 9.525 x 300-1400; 10 x 100-2900; 12 x 100-2900; 12.7 x 100-1200; 13 x 100-1900; 14 x 100-2000; 15 x 100-1900; 15.875 x 100-2000; 19.05 x 100-1800; 20 x 100-2100; 22.225 x 100-1700; 25 x 100-2100; 30 x 100-1900 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 - 18 % Show Supplier Material materials with Dehnung of 10 - 18 % |
Härte, Vickers, 10 | 23.0 °C | 215 - 280 [-] Show Supplier Material materials with Härte, Vickers, 10 of 215 - 280 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 380 - 515 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 380 - 515 MPa |
Zugfestigkeit | 23.0 °C | 515 - 620 MPa Show Supplier Material materials with Zugfestigkeit of 515 - 620 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2620 °C Show Supplier Material materials with Schmelzpunkt of 2620 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.39 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.39 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | 99.97 % Show Supplier Material materials with Molybdän of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 6E-4 % Show Supplier Material materials with Sauerstoff of 6E-4 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |