Allgemein
Abmessung
Property | Value |
---|---|
Durchmesser | 140 - 165 mm Show Supplier Material materials with Durchmesser of 140 - 165 mm |
Länge | 100 - 500 mm Show Supplier Material materials with Länge of 100 - 500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 140 x 100-500; 165 x 100-500 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % |
Härte, Vickers, 10 | 23.0 °C | 180 - 240 [-] Show Supplier Material materials with Härte, Vickers, 10 of 180 - 240 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 380 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 380 MPa |
Zugfestigkeit | 23.0 °C | 450 MPa Show Supplier Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2620 °C Show Supplier Material materials with Schmelzpunkt of 2620 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.39 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.39 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | 99.97 % Show Supplier Material materials with Molybdän of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 6E-4 % Show Supplier Material materials with Sauerstoff of 6E-4 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |