Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Dichte of 10.2 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Oberflächenrauigkeit | 1 μm Show Supplier Material materials with Oberflächenrauigkeit of 1 μm |
Abmessung
Property | Value |
---|---|
Breite | 600 - 750 mm Show Supplier Material materials with Breite of 600 - 750 mm |
Dicke | 0.2 - 3 mm Show Supplier Material materials with Dicke of 0.2 - 3 mm |
Länge | 1600 - 2000 mm Show Supplier Material materials with Länge of 1600 - 2000 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 600 x 2000 x 0.2; 600 x 2000 x 0.3; 600 x 2000 x 0.5; 750 x 2000 x 1; 750 x 2300 x 1.5; 750 x 2000 x 2; 750 x 2000 x 2.5; 750 x 1600 x 3 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 - 15 % Show Supplier Material materials with Dehnung of 2 - 15 % |
Härte, Vickers | 23.0 °C | 240 - 280 [-] Show Supplier Material materials with Härte, Vickers of 240 - 280 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 620 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 620 MPa |
Zugfestigkeit | 23.0 °C | 640 - 700 MPa Show Supplier Material materials with Zugfestigkeit of 640 - 700 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2620 °C Show Supplier Material materials with Schmelzpunkt of 2620 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.39 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.39 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | 99.97 % Show Supplier Material materials with Molybdän of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 6E-4 % Show Supplier Material materials with Sauerstoff of 6E-4 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |