Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Dichte of 10.2 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Abmessung
Property | Value |
---|---|
Durchmesser | 0.5 - 1 mm Show Supplier Material materials with Durchmesser of 0.5 - 1 mm |
Dimensions | Available diameters (mm): 0.5; 1 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % |
Zugfestigkeit | 23.0 °C | 750 - 1200 MPa Show Supplier Material materials with Zugfestigkeit of 750 - 1200 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2620 °C Show Supplier Material materials with Schmelzpunkt of 2620 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.39 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.39 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | 99.97 % Show Supplier Material materials with Molybdän of 99.97 % |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 6E-4 % Show Supplier Material materials with Sauerstoff of 6E-4 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Molybdenum-wire is used in a wide variety of high temperature applications. Typical applications are the lighting industry, conductor elements and fabric components in furnace construction and special applications. |