Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.2 g/cm³ Show Supplier Material materials with Dichte of 10.2 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 0.5 - 0.8 mm Show Supplier Material materials with Durchmesser of 0.5 - 0.8 mm |
Dimensions | Available diameters (mm): 0.5; 0.4; 0.6; 0.7; 0.8 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % |
Zugfestigkeit | 23.0 °C | 970 - 1150 MPa Show Supplier Material materials with Zugfestigkeit of 970 - 1150 MPa |
Thermisch
Property | Value |
---|---|
Kristallisationstemperatur | 1700 °C Show Supplier Material materials with Kristallisationstemperatur of 1700 °C |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % | ||
Andere | 0.22 - 0.36 % Show Supplier Material materials with Andere of 0.22 - 0.36 % | as La₂O₃ | |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | ||
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % | ||
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % | ||
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % | ||
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % | ||
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % | ||
Lanthan | 0.19 - 0.31 % Show Supplier Material materials with Lanthan of 0.19 - 0.31 % | as La | |
Molybdän | balance | ||
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % | ||
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % | ||
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % | ||
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | This alloy is mostly machined to produce furnace components such as stranded and other wires, sintering and annealing boats or evaporator coils. In the lighting industry, molybdenum-lanthanum oxide is used, for example, for retaining and feed wires. |